Web15 de dez. de 2011 · Polycrystalline Cr-doped higher manganese silicides (HMSs) Mn 1−x Cr x Si 1.80 (x = 0 to 0.03) were prepared by the in situ spark plasma sintering method. The phase structure and microstructure of the bulk samples were investigated, and their thermoelectric (TE) properties were measured from 473 K to 873 K. x-Ray diffraction … Web1 de jun. de 2024 · Higher manganese silicide (HMS) is a P-type medium temperature thermoelectric (TE) material, which has attracted widespread attention over the past …
Thermoelectric Properties of Higher Manganese Silicides …
Web1 de abr. de 2024 · Download Citation On Apr 1, 2024, Zhiliang Li and others published Isoelectronic Re-Ge-Codoped Higher Manganese Silicides with Enhanced Thermoelectric Properties via Band Optimization, Charge ... Web1 de ago. de 2024 · Herein, higher manganese silicides (HMS) are decorated on carbon coated silicon, denoted as [email protected]@C, by coating microscale waste Si powders recovered from photovoltaic industry with in situ polymerized resorcinol formaldehyde (RF) resin, followed by absorbing manganese acetate tetrahydrate and thermal pyrolizing in … small business owner quotes
Ab initio study of the band structures of different phases of higher …
Web25 de ago. de 2011 · Rhenium-doped higher manganese silicide based materials have been prepared by hot pressing. It has been shown that the pressing temperature of the materials can be lowered by adding titanium as a reductant or by sonication during pressing. The average thermoelectric figure of merit of the materials in the temperature range … Web21 de nov. de 2016 · 55, 56 Higher manganese silicides, exemplified by MnSi 1.70+ with = 0.01-0.05, represent a series of Nowotny chimney-ladder phases, consisting of a square-arranged Mn sublattice and a "ladder ... Web2 de jun. de 2015 · An easy and efficient process involving ball milling under soft conditions and spark plasma sintering was used to synthesize higher manganese silicide (HMS)-based compounds, for example MnSi 1.75 Ge 0.02, with different molybdenum, tungsten, and aluminium substitution.The x-ray diffraction patterns of the samples after sintering … small business owner resume responsibilities